This is a Demo Server. Data inside this system is only for test purpose.
 

Sintering, co-sintering and microstructure control of oxide based materials: Zirconia, alumina, spinel, alumina-zirconia and spinel-alumina

dc.contributor.advisor Akkurt, Sedat en
dc.contributor.author Yalamaç, Emre
dc.date.accessioned 2023-11-16T12:03:26Z
dc.date.available 2023-11-16T12:03:26Z
dc.date.issued 2010 en
dc.department Mechanical Engineering en_US
dc.description Thesis (Doctoral)--Izmir Institute of Technology, Mechanical Engineering, Izmir, 2010 en
dc.description Includes bibliographical references (leaves: 148-157) en
dc.description Text in English; Abstract: Turkish and English en
dc.description xxi, 157 leaves en
dc.description.abstract Densification and microstructural evolution during co-sintering of alumina (Al2O3) . zirconia (Y-ZrO2) and alumina . spinel (MgAl2O4) co-pressed bimaterials were investigated. First high purity submicron powders of monomaterials of alumina, spinel and zirconia were pressed at 100 to 250 MPa with different dry pressing techniques like UP (uniaxial pressing) and CIP (cold isostatic pressing). The latter was found to provide higher green densities. Before co-sintering of bi-materials, sintering behaviors of their end-members were studied by vertical dilatometer to determine the degree of shrinkage mismatches between the end-members. The effects of precoarsening and two-step sintering on the densification and microstructure of spinel ceramics were tested. Samples were etched both chemically and thermally to better understand their structure. Crack-free bonds were observed in alumina-spinel bi-materials after compaction by UP+CIP. Interfaces between alumina and spinel after treatment at 1400-1500 C were investigated by SEM, EDS, WDS, EBSD. A spinel interlayer with columnar grains of up to 40 .m length and 5 .m width was observed after 16 hours at 1500 C. Growth rate of this interlayer from spinel toward alumina was found to follow parabolic kinetics, controlled by a diffusion mechanism of probably lattice diffusion of O2- ions. Two isothermal steps co-sintering at 1400 C and 1500 C on the interlayer formation was tested. Two separate areas formed in the interlayer spinel. Diffusion couple tests of spinel and alumina produced the same columnar spinel grains at the interface with the same kinetics as in co-sintering experiments. Phase boundaries between the columnar spinel and alumina grains had a characteristic center of curvature located in alumina which was further indication of the direction of growth of the interlayer. en
dc.identifier.uri http://standard-demo.gcris.com/handle/123456789/6068
dc.language.iso en en_US
dc.oaire.dateofacceptance 2010-01-01
dc.oaire.impulse 0
dc.oaire.influence 2.9837197E-9
dc.oaire.influence_alt 0
dc.oaire.is_green true
dc.oaire.isindiamondjournal false
dc.oaire.keywords Mechanical Engineering
dc.oaire.keywords Makine Mühendisliği
dc.oaire.keywords Material science
dc.oaire.popularity 6.5821576E-10
dc.oaire.popularity_alt 0.0
dc.oaire.publiclyfunded false
dc.publisher Izmir Institute of Technology en
dc.relation.publicationcategory Tez en_US
dc.rights info:eu-repo/semantics/openAccess en_US
dc.subject.lcsh Sintering en
dc.subject.lcsh Microstructure en
dc.subject.lcsh Zirconium oxide en
dc.subject.lcsh Zirconium alloys en
dc.subject.lcsh Aluminum oxide en
dc.subject.lcsh Spinel en
dc.title Sintering, co-sintering and microstructure control of oxide based materials: Zirconia, alumina, spinel, alumina-zirconia and spinel-alumina en_US