The deterioration of historic buildings and monuments constructed by marble has been accelerated in the past century due to the effects of air pollution. The main pollutant Sulphur dioxide (SO2) reacts with marble composed primarily of calcite (CaCO3), the firs step of decay which called gypsum (CaSO4.2H2O) crust is formed and this process can be accelerated when the surfaces exposed to the rain.In this study, the possibilities of slowing down the SO2-marble reactions were investigated by coating the surface of marble with some bio-degradable polymers: zein, chitosan, polyhydroxybutyrate (PHB) and polylactic acid (PLA) as protective agents.Uncoated control marbles and biodegradable polymer coated marbles were exposed at nearly 8 ppm SO2 concentration at 100 % relative humidity conditions in a reaction chamber for several days. The extent of reaction was determined by leaching sulphate from the marble surface into deionized water and measuring the total concentration of sulphate with ion chromatography (IC). Then, gypsum crust thickness, polymers % protection factor and average deposition velocity were calculated. Concurrently, the ratio and amount of calcium sulfite hemihydrate (CaSO3.H2O)and gypsum (CaSO4.2H2O) were determined by FT-IR analysis. The surface morphology of SO2 exposed marble to distinguished calcium sulfite hemihydrate and gypsum crystals were determined by Scanning Electron Microscope (SEM).The results of the study showed that SO2-calcite reaction increased in the use of zein, glycerol added zein and chitosan polymers on the surface of marble. While, PHB treated marble surfaces had 5 % increases in the protection factor. The low molecular weight PLA protection factor was 45 % after 85 days exposure. Similar results were observed when the high molecular weight of PLA used. The protection was extended to more than 90 days having 60 % protection factor.

Description

Thesis (Master)--Izmir Institute of Technology, Environmental Engineering, Izmir, 2007
Includes bibliographical references (leaves: 72-77)
Text in English; Abstract: Turkish and English
xiii, 89 leaves

Keywords

Environmental Engineering, Çevre Mühendisliği, Architecture, Mimarlık, Chemical Engineering, TA428.M3 O151 2007, Kimya Mühendisliği

Turkish CoHE Thesis Center URL

Fields of Science

Citation

WoS Q

Scopus Q

Source

Volume

Issue

Start Page

End Page

Collections

Google Scholar Logo
Google Scholar™

Sustainable Development Goals

SDG data could not be loaded because of an error. Please refresh the page or try again later.